In nanopore technology, the development of multiplexed detection and release platforms with high spatial and temporal resolution remains a significant challenge due to the difficulty in distinguishing signals originating from different nanopores in a single chip. In this work, we present a solid-state nanopore system functionalized with molecularly imprinted polymers (MIPs) for the selective detection and controlled release of neurotransmitters. We designed a nanopore array where each nanopore is functionalized with a specific MIP able to recognize specific neurotransmitters (dopamine, gamma-aminobutyric acid, and histamine, respectively). The platform demonstrated high performance in terms of sensitivity, selectivity, recovery, and stability. Multiplexed detection with high spatiotemporal resolution of the order of 100 ms/ 3 μm was achieved by specifically depositing MIPs and conductive hydrogels on different nanopores prepared on a single solid-state membrane. The employment of micro-chambers for each nanopore prevented signal cross-talk, thereby enabling simultaneous detection and release of multiple neurotransmitters. Moreover, we demonstrated computing with different logic gates and in-edge computing. This nanopore platform represents a radically novel approach towards hybrid solid-state nanopores able to perform real-time label-free multiplex detection, controlled biomolecule release, and ionic logic computing, addressing key challenges in neurochemical sensing and bio-computation.
academicMolecularly imprinted nanopores for multiplexed sensing, release, and in-edge computing
- 论文ID: 2510.13490
- 标题: Molecularly imprinted nanopores for multiplexed sensing, release, and in-edge computing
- 作者: Ali Douaki, Shukun Weng, Silvia Dante, Nako Nakatsuka, Makusu Tsutsui, Roman Krahne, Denis Garoli
- 分类: physics.app-ph (应用物理)
- 机构: 意大利技术研究所、洛桑联邦理工学院、大阪大学、摩德纳大学
- 论文链接: https://arxiv.org/abs/2510.13490
本研究提出了一种基于分子印迹聚合物(MIPs)功能化的固态纳米孔系统,用于神经递质的选择性检测和可控释放。研究团队设计了纳米孔阵列,每个纳米孔都用特定的MIP功能化,能够识别特定的神经递质(多巴胺、γ-氨基丁酸和组胺)。该平台在灵敏度、选择性、回收率和稳定性方面表现出色,实现了约100毫秒/3微米的高时空分辨率多路检测,并展示了逻辑门运算和边缘计算能力。
纳米孔技术中,开发具有高时空分辨率的多路检测和释放平台仍然是一个重大挑战,主要困难在于难以区分来自单一芯片上不同纳米孔的信号。
- 神经科学需求: 多巴胺、GABA和组胺等神经递质在大脑功能中起关键作用,其失调与抑郁症、帕金森病和精神分裂症等疾病相关
- 生物过程监测: 许多生物过程发生在高度受限的空间内,时间尺度为毫秒到几十毫秒,需要高时空分辨率的检测平台
- 实时多路检测: 同时监测多种神经递质水平对理解复杂神经过程至关重要
- 传统检测方法: 基于电化学和光学方法的传统检测在时空分辨率、工作复杂性和选择性方面存在不足
- 信号串扰: 多路系统中难以区分来自不同纳米孔的信号,影响测量和控制精度
- 缺乏集成: 现有系统缺乏将传感、计算和释放功能集成在单一平台上的能力
- 首次实现MIP-纳米孔集成: 开发了首个将分子印迹聚合物与固态纳米孔集成的多路传感平台
- 解决信号串扰问题: 通过导电水凝胶微室技术实现了独立的电流测量,防止信号串扰
- 多功能集成平台: 实现了传感、可控释放和离子逻辑计算的三重功能集成
- 高性能检测: 实现了皮摩尔级别的检测限(多巴胺2.82 pM, GABA 1.99 pM, 组胺2 nM)
- 边缘计算能力: 首次展示了基于神经递质的逻辑门(NOT、NOR、NAND)和边缘计算
构建一个能够同时进行多种神经递质的实时检测、可控释放和逻辑计算的集成纳米孔平台。
- 纳米孔制备: 使用聚焦离子束(FIB)在Si₃N₄膜上制备直径40±10 nm的纳米孔
- 表面功能化: 通过原子层沉积进行APTES涂层处理
- MIP合成: 采用原位聚合法,以甲基丙烯酸(MAA)、丙烯酰胺(ACM)和交联剂MBAA按1:2:2:10摩尔比合成
- 空间分离: 在单一Si₃N₄膜上制备三个功能化不同MIP的纳米孔
- 导电水凝胶微室: 使用聚乙烯醇-海藻酸钠复合水凝胶作为独立的离子传输通道
- 防串扰机制: 共享顺式室,独立反式室的设计避免信号干扰
- 检测原理: 目标分子与MIP结合导致纳米孔部分阻塞,离子电流减少
- 释放机制: 通过电场辅助静电解吸实现分子的可控释放
- 逻辑运算: 基于神经递质存在/不存在的二进制输入实现逻辑门功能
- 分子印迹技术与纳米孔的首次结合: 利用MIP的高选择性解决了纳米孔传感器的特异性问题
- 导电水凝胶微室技术: 创新性地解决了多路系统中的信号串扰问题
- 电场辅助释放机制: 通过局部电势降(约0.1V)实现快速可控的分子释放
- 生物逻辑计算: 首次实现基于神经递质的离子逻辑运算
- 缓冲液: 1× PBS (137 mM NaCl, 2.7 mM KCl, 10 mM Na₂HPO₄, 1.8 mM KH₂PO₄, pH 7.4)
- 目标分子: 多巴胺、GABA、组胺
- 复杂介质: 神经基础培养基(neurobasal medium)
- 形貌表征: SEM、AFM
- 光谱分析: UV-Vis分光光度法
- 动力学分析: 石英晶体微天平(QCM-D)
- 电学测量: 离子电导测量
- 灵敏度: 检测限(LOD)和定量限(LOQ)
- 选择性: 对结构类似物的交叉反应性
- 稳定性: 长期存储稳定性和重复使用性
- 时空分辨率: 响应时间和空间分辨率
- 检测范围: 1 pM - 100 μM
- 检测限: 2.82 pM (LOD), 23.20 pM (LOQ)
- 选择性: 对去甲肾上腺素和血清素的交叉反应性分别为5.75±0.56%和3.75±0.2%
- 稳定性: 6次循环后保持95%以上的初始灵敏度,9天内保持97.2±7.0%的响应
- 检测范围: 0.1 nM - 100 mM
- 检测限: 1.99 pM
- 线性度: R² = 0.96
- 稳定性: 15次循环后保持92%的初始灵敏度
- 检测范围: 1 nM - 100 mM
- 检测限: 2 nM
- 线性度: R² = 0.97
- 稳定性: 15次循环后保持90%的初始灵敏度,30天内性能稳定
- 时空分辨率: ~100 ms / 3 μm
- 选择性检测: 每个纳米孔仅对其特定目标产生显著响应(~25-30%电流减少)
- 防串扰: 成功实现独立信号测量
- 释放效率: 5次脉冲后约80%的载药分子被释放
- 释放机制: 电场辅助静电解吸,局部电势降约0.1V
- 可逆性: 6次检测-释放循环验证了平台的可逆操作能力
成功实现了NOT、NOR和NAND逻辑门操作,为生物计算和神经形态系统提供了新的可能性。
纳米孔技术因其高灵敏度、无标记检测、实时监测等优势成为最有前景的技术之一,但多路无标记检测仍是挑战。
MIPs在电化学传感器和场效应晶体管中已显示出增强选择性的巨大潜力,但与纳米孔的结合此前基本未被探索。
已在电阻器件、光子系统、交叉阵列等多个平台成功实现,但传感和计算在单一存储单元中的完全实验集成仍大部分未被探索。
- 成功开发了首个MIP功能化纳米孔多路传感平台
- 实现了皮摩尔级别的高灵敏度检测
- 通过导电水凝胶技术解决了信号串扰问题
- 展示了传感、释放和逻辑计算的三重功能集成
- 为神经化学监测和生物计算提供了新的技术途径
- 复杂介质影响: 在神经基础培养基中的响应略低于PBS缓冲液
- 温度敏感性: 需要在特定温度条件下操作
- 长期稳定性: 虽然表现良好,但仍需更长期的稳定性验证
- 制备复杂性: 需要精密的微加工和化学合成技术
- 扩展目标分子种类: 开发更多种类神经递质的MIP传感器
- 提高集成度: 增加单芯片上的纳米孔数量
- 在体应用: 开发适用于活体检测的微型化系统
- 智能算法: 结合机器学习算法提高检测精度和预测能力
- 首创性集成: 首次将MIP技术与纳米孔传感相结合,开创了新的研究方向
- 工程解决方案: 导电水凝胶微室技术巧妙解决了多路系统的信号串扰问题
- 多功能集成: 在单一平台上实现传感、释放和计算的集成,具有重要的技术价值
- 全面表征: 从单一传感器到多路系统,从材料表征到功能验证,实验设计完整
- 性能优异: 检测限达到皮摩尔级别,满足生理相关浓度的检测需求
- 机理阐释: 通过QCM-D、温度实验等深入探讨了释放机理
- 神经科学应用: 为神经递质的实时监测提供了新工具
- 生物计算: 开辟了基于生物分子的逻辑计算新领域
- 智能药物释放: 为精准医疗提供了新的技术平台
- 制备复杂性: 需要多步精密加工,可能影响批量生产和标准化
- 环境敏感性: 对pH、温度等环境条件较为敏感
- 交叉反应: 虽然选择性良好,但仍存在一定程度的交叉反应
- 生物相关性: 主要在缓冲液中进行测试,与真实生物环境存在差距
- 长期稳定性: 虽然进行了9-30天的测试,但对于实际应用可能需要更长期的验证
- 通量限制: 目前仅展示了3个纳米孔的集成,扩展性有待验证
- 跨学科融合: 将材料科学、纳米技术、生物传感和计算科学有机结合
- 方法学创新: 为纳米孔传感技术提供了新的功能化策略
- 理论深化: 对电场辅助分子解吸机理进行了深入的理论分析
- 医疗诊断: 可用于神经系统疾病的早期诊断和监测
- 药物开发: 为神经药物的筛选和评价提供新工具
- 生物工程: 为合成生物学和生物计算提供硬件基础
论文提供了详细的材料制备、实验方法和数据分析过程,具有良好的可复现性。
- 神经科学研究: 用于神经递质动力学研究
- 临床诊断: 神经系统疾病的生物标志物检测
- 药物筛选: 神经活性药物的效果评价
- 生物计算: 分子逻辑电路的构建
- 智能材料: 响应性药物释放系统
论文引用了80篇相关文献,涵盖了纳米孔技术、分子印迹、神经科学、生物传感和计算科学等多个领域的重要工作,为研究提供了坚实的理论基础。
总体评价: 这是一篇具有重要创新意义的跨学科研究论文,成功地将分子印迹技术与纳米孔传感相结合,实现了多功能集成的生物传感平台。论文在技术创新、实验验证和应用前景方面都表现出色,为纳米生物传感和生物计算领域的发展做出了重要贡献。尽管存在一些技术挑战和应用局限,但其开创性的工作为未来的研究和应用奠定了重要基础。